Select Page


Battery was starting to show its age. It was very sluggish at cranking the old V8. The battery was fully charge by a battery charger and left to sit for 36hrs before the testing began. After adding epsom salt/distilled water and charging then slightly discharging 3 times the battery works a lot better. Duralast Gold Manufactured: March 2003 film date 1-23-2011 Initial testing: 44.6 F degrees 12.38 volts-Static 11.03 volts-5 sec 100amp load 10.99 volts-10 sec 100amp load 10.96 volts-15 sec 100amp load 11.97 volts-5 sec after let off 100 amp load 12.05 volts-10 sec after let off 100 amp load 12.09 volts-15 sec after let off 100 amp load After 60cc/4TBS Epsom Salt and 36hr rest 43.5 F Degrees 12.72 volts-Static 11.29 volts-5 sec 100amp load 11.25 volts-10 sec 100amp load 11.26 volts-15 sec 100amp load 12.13 volts-5 sec after let off 100 amp load 12.19 volts-10 sec after let off 100 amp load 12.23 volts-15 sec after let off 100 amp load